Amacandelo amabini e-polyamide adduct aphilisiwe, i-solids ephezulu, ipeyinti ephezulu ye-epoxy enokumelana kakuhle namanzi, i-oyile, iikhemikhali, kunye nefuthe kunye neempawu zokumelana ne-abrasion.
Iimbonakalo
1.Ukuchasana kwamanzi okugqwesileyo kunye nokuxhathisa umhlwa.
I-2.Ukumelana neekhemikhali ezilungileyo kunye nokuxhathisa ioli.
I-3.Ukubambelela kakuhle, ukuchasana kwempembelelo, ukuxhatshazwa kokugqoka
Usetyenziso olucetyiswayo
Ukukhusela intsimbi kunye nekhonkrithi kwiindawo ezinobungozi kakhulu, zingasetyenziselwa njengengubo ephakathi okanye njengengubo ephezulu yezakhiwo zangaphakathi.
Imiyalelo yesicelo
I-Substrate kunye nonyango lwangaphezulu
Sintsimbi:uqhushumbo lucocwe ukuya ku-Sa2.5 (ISO8501-1) okanye ubuncinci be-SSPC SP-6, iprofayili yokuqhushumba Rz50μm~100μm (ISO8503-1) okanye isixhobo samandla sicocwe kubuncinci be-ISO-St3.0/SSPC SP3
Yonke imiphezulu eza kugqunywa iya kucoceka, yome kwaye ingabi nabumdaka, kwaye iya kuvavanywa kwaye iphathwe ngokuhambelana ne-ISO8504.
Isiseko seworkshop esakhiwe ngaphambili:I-Welds, i-firework calibration kunye nomonakalo kufuneka iqhume icocwe kwi-Sa2.5 (ISO8501-1), okanye isixhobo samandla sicocwe ukuya kwi-St3.0.
Tyho phezulu:Susa ngokucokisekileyo igrisi kumphezulu kwaye ucoce ityuwa kunye nobunye ukungcola.
Cumphezulu oncrete:Ukufaka i-sealer efanelekileyo yokutywina i-pores yomhlaba ngaphambi kokufaka isicelo.
Oumphezulu:nceda uqhagamshelane ne-ZINDN.
Iyasebenza kwaye iyanyangwa
● Ubushushu bemo engqongileyo kufuneka bube ukusuka kwi-5℃ ukuya kwi-38℃, ukufuma komoya okunxulumeneyo akufunekanga kube ngaphezu kwe-85%.
● Ubushushu be-substrate ngexesha lokufakwa kunye nokunyanga kufuneka lube yi-3℃ ngaphezu kwendawo yombethe.
● Ukusetyenziswa kwangaphandle akuvumelekanga kwimozulu embi njengemvula, inkungu, ikhephu, umoya onamandla kunye nothuli olunzima.
Ubomi bembiza
5℃ | 15℃ | 25℃ | 35℃ |
Iiyure ezi-4 | Iiyure ezi-3 | Iiyure ezi-2 | 1.5 iiyure |
Iindlela zokusetyenziswa
Isitshizi esingenamoya, isitshizi somoya asikhuthazwa.
I-brush kunye ne-roller yokugqoka inconywa kuphela ngengubo yomgca, ukugubungela indawo encinci okanye ukulungiswa.
Iiparamitha zesicelo
Indlela yokusetyenziswa | Iyunithi | Isitshizi esingenamoya | Ibrashi/iRola |
Nozzle orifice | mm | 0.43-0.53 | —- |
Uxinzelelo lombhobho | kg/cm2 | 150 ~ 200 | —- |
Thinner | % | 0~10 | 5~10 |
Ukomisa kunye nokuNyanga
Umphezulu we-Substrate ubushushu | 5℃ | 15℃ | 25℃ | 35℃ |
Umphezulu-womile | Iiyure ezili-16. | Iiyure ezisi-8. | Iiyure ezi-4. | Iiyure ezi-2. |
Ngoma | Iiyure ezingama-48. | Iiyure ezingama-24. | 12hrs. | Iiyure ezi-6. |
Uphiliswe ngokupheleleyo | Iintsuku ezili-14 | Iintsuku ezili-10 | Iintsuku ezi-6 | Iintsuku ezi-4 |
Ixesha lekhefu lokuhlaziya (Um.) | Iiyure ezingama-48 | Iiyure ezingama-24. | 12hrs. | Iiyure ezi-6. |
Ixesha lokuphumla kwakhona (Ubuninzi.) (no.2 umaleko) | Iintsuku ezili-14 | Iintsuku ezili-10 | Iintsuku ezi-6 | Iintsuku ezi-4 |
Ixesha lekhefu lokubuyisela kwakhona (ubuninzi.) (Idyasi ephezulu) | Iintsuku ezingama-30 | Iintsuku ezingama-20 | Iintsuku ezili-14 | Iintsuku ezisi-7 |
Ukwaleka okwandulelayo kunye nesiphumo
Idyasi eyandulelayo:I-Epoxy zinc phosphate, i-Epoxy zinc ecebileyo, i-Epoxy primer, inokuthi isetyenziswe ngokuthe ngqo kwi-steel surface blast ecociweyo kwi-Sa2.5 (ISO8501-1).
Idyasi yesiphumo:Epoxy topcoat, Polyurethane, Fluorocarbon, Polysiloxane... etc
Ukupakisha kunye noGcino
Ukupakisha:isiseko 24kg, iarhente yokunyanga 4kg
Indawo yokuflasha:>25℃(Umxube)
Ugcino :Kufuneka igcinwe ngokuhambelana nemigaqo yorhulumente wasekhaya.Indawo yokugcina kufuneka yomile, ipholile, ingene umoya kwaye ingabikho kubushushu kunye nemithombo yomlilo.Isingxobo sokupakisha kufuneka sigcinwe sivalwe ngci.
Beka ubomi kwishelufa:Unyaka we-1 phantsi kweemeko ezilungileyo zokugcina ukusuka kwixesha lokuvelisa.