Icandelo elinye elinomxholo ophezulu we-zinc kunye nefuthe lesilivere, elisetyenziswe ngumaleko omnye okanye i-topcoat ene-zindn ebandayo ye-galvanizing
Iimbonakalo
Uthuli lwe-1.Zinc lusetyenziswa kunye ne-flake aluminium powder, umphumo wesinyithi ulungile;I-flake ye-aluminium powder ihlelwe ngokuhambelana nefilimu yokugqoka, enokuthintela ukungena komswakama kunye nemisebe ye-ultraviolet kwifilimu yokugqoka.
2.Isicelo esiluncedo kunye ne-Eco-friendly
3.Umsebenzi ogqwesileyo wokuchasana nokuguquka kwemibala kwimvula yangaphandle
Isiqulatho sothuli lweZinc≥80%, umgubo wealuminium≥10%
Usetyenziso olucetyiswayo
Ulwakhiwo lwensimbi ixesha elide leenjongo zokuchasana nomhlwa, lunokusetyenziswa njengedyasi enye, kwaye lunokusetyenziswa njengedyasi ephezulu kunye nekhompawundi ebandayo ye-ZD.
Ukucofa kwesakhiwo sentsimbi, esona sixhobo silungileyo sokubuyisela okanye ukucofa isitshizi segalvanized kunye ne-hot-dip galvanized layers.
Imiyalelo yesicelo
Isubstrate esebenzayo kunye noNyango loMphezulu:
Intsimbi: uqhushumbo lucocwe ukuya ku-Sa2.5 (ISO8501-1) okanye ubuncinci be-SSPC SP-6, iprofayili yokuqhushumba Rz40μm~75μm (ISO8503-1) okanye isixhobo samandla sicocwe kubuncinci be-ISO-St3.0/SSPC SP3
Ukuchukumisa umphezulu owenziwe ngegalvanized
Susa ngokucokisekileyo igrisi phezu komhlaba nge-agent yokucoca, ucoce ityuwa kunye nolunye ukungcola ngokusebenzisa amanzi ahlambulukileyo aphezulu, sebenzisa isixhobo samandla ukupolisha indawo ye-rust okanye i-mill scale.
Iyasebenza kwaye iyanyangwa
Ubomi bembiza:mda
Ubushushu bemeko yesicelo:0℃-50℃
Ukufuma komoya okunxulumeneyo:≤95%
Ubushushu be-substrate ngexesha lokufakwa kunye nokunyanga kufuneka bube yi-3℃ ngaphezu kwendawo yombethe
Ukusetyenziswa kwangaphandle akuvumelekanga kwimozulu embi njengemvula, inkungu, ikhephu, umoya onamandla kunye nothuli olunzima
Iqondo lobushushu liphezulu ehlotyeni, lumka xa utshiza okomileyo, kwaye gcina umoya wakho ungenile ngexesha lokugalela kunye namaxesha okomisa kwiindawo ezimxinwa.
Iindlela zokusetyenziswa
Isitshizi esingenamoya/isitshizi somoya/ibrashi/irola
Ibhrashi kunye ne-roller yokwambathisa zicetyiswa kuphela ngedyasi enemigca, indawo encinci yokwaleka okanye ubambe phezulu kwaye kunokubangela umahluko wombala.
Iiparamitha zeSicelo
Indlela yokusetyenziswa | Iyunithi | Isitshizi esingenamoya | Isitshizi somoya | Ibrashi/iRola |
Nozzle orifice | mm | 0.43-0.53 | 1.5–2.5 | —- |
Uxinzelelo lombhobho: | kg/cm2 | 150 ~ 200 | 3~4 | —- |
Thinner | % | 5~10 | 10~20 | 0~10 |
Ukomisa kunye nokuNyanga
Ubushushu be-substrate | 5℃ | 15℃ | 25℃ | 35℃ |
Umphezulu-womile | Iiyure ezi-2. | Iyure e-1. | 30 imiz | 10 imiz |
Ngoma | 5 iiyure. | Iiyure ezi-4 | Iiyure ezi-2. | Iyure e-1. |
Isithuba sokubuyisela kwakhona uMz. | 5 iiyure. | Iiyure ezi-4 | Iiyure ezi-2. | Iyure e-1. |
Recoating interval Max. | Ukubuyisela kwakhona akunamda, indawo edibeneyo kufuneka ikhululeke kwi-chalking kunye nezinye izinto ezingcolileyo.Yigcine icocekile kwaye yomile.Ukuba kuyimfuneko, yenza i-roughening ngokwaneleyo ngaphambi kokutyabeka. |
Ukwaleka okwandulelayo kunye nesiphumo
Idyasi eyandulelayo:I-ZD Cold Galvanizing, okanye utshize ngokuthe ngqo phezu kwentsimbi okanye i-hot-dip galvanized okanye i-hot-sprayed steel kunye nonyango oluphezulu lwe-Sa2.5 okanye i-St3.
Idyasi yesiphumo:Kwiimeko eziqhelekileyo, akukho mfuneko yokwaleka ngenxa yoko.
Ukupakisha kunye noGcino
Ukupakisha:25kg
Indawo yokuflasha:>27℃
Ugcino:Kufuneka igcinwe ngokuhambelana nemigaqo yorhulumente wasekhaya.Indawo yokugcina kufuneka yomile, ipholile, ingene umoya kwaye ingabikho kubushushu nakwimithombo yomlilo.Isingxobo sokupakisha kufuneka sigcinwe sivalwe ngci.
Beka ubomi kwishelufa:Iminyaka emi-2 ikwimeko entle yokugcina.